文件名称:快速沉淀法制备多孔纳米NiO及其电容性质研究 (2006年)
文件大小:300KB
文件格式:PDF
更新时间:2024-05-19 00:15:57
自然科学 论文
Ni (OH)2 with a high specific surface area was synthesized by a facile fast precipitation method. Porous nano-NiO was obtained by calcining Ni (OH)2 at 300℃. The NiO sample possesses a fine porous distribution at around 3—10nm. The BET specific surface ar